Preparation and Testing of Cold Cream
To prepare a cold cream and test its pH, spreadability and stability.
Theoretical Foundations
Cold cream is a water-in-oil emulsion of mineral oil and waxes stabilised by borax-beeswax soap. The borax saponifies some beeswax acids in situ, forming the emulsifier. Quality tests include pH (5.5-7 for skin compatibility), spreadability (slip), and emulsion stability on centrifugation and thermal cycling.
Required Apparatus & Chemicals
Laboratory Apparatus
- Water bath
- Beakers
- Glass rod / homogeniser
- pH meter or strips
- Centrifuge tubes
- Glass slides
Chemical Reagents
- Beeswax (12 g)
- Mineral oil (50 mL)
- Borax (0.8 g)
- Distilled water (28 mL)
- Perfume (few drops, optional)
Step-by-Step Practical Procedure
- Melt beeswax in mineral oil on a water bath at 70 C (oil phase).
- Dissolve borax in distilled water at 70 C (aqueous phase).
- Add the aqueous phase to the oil phase slowly with vigorous stirring.
- Stir until cool to form a smooth cream; add perfume below 40 C.
- Measure pH of a 10% dispersion.
- Test spreadability by pressing 1 g between glass slides under a weight and measuring the spread diameter.
- Centrifuge a sample at 3000 rpm for 30 minutes and check for water separation.
Observations & Expected Results
A good cream is glossy, homogeneous, pH 6-7, spreads evenly and shows no water separation after centrifugation.
Worked Stoichiometric Calculations
Problem: 1 g of cream spread to a circle of diameter 6.0 cm under the standard weight; a reference cream spreads to 5.0 cm. Which spreads more easily and by what area ratio?
Working: Area ratio = (6.0/5.0)^2 = 1.44. The prepared cream spreads 1.44 times more easily than the reference.
Safety Precautions & Hazard Control
- Keep both phases at the same temperature when mixing or the emulsion breaks.
- Add water to oil slowly with continuous stirring.
- Do not overheat beeswax; it darkens and smells burnt.
- Check pH; free borax above pH 8 irritates skin.
Waste Disposal Protocol
Small cosmetic residues can go to solid waste; wash glassware with detergent.
Viva Voce Oral Defense Questions & Answers
Q: What emulsifier forms in cold cream?
A: Sodium salts of beeswax fatty acids, formed when borax reacts with the free acids in beeswax during mixing.
Q: Why is it called cold cream?
A: The traditional formula feels cool on skin because its water phase evaporates after application.