Nickel Determination: Dimethylglyoxime Extraction at 465 nm
To determine nickel by extracting the red Ni(DMG)2 complex into chloroform and measuring at 465 nm.
Theoretical Foundations
Dimethylglyoxime gives the scarlet-red chelate Ni(DMG)2 with Ni²⁺ in ammoniacal solution (λmax ≈ 465 nm in chloroform, ε ≈ 1.7 × 10⁴ L mol⁻¹ cm⁻¹). Extraction into chloroform separates nickel from interfering ions and concentrates the colour, giving a sensitive spectrophotometric finish.
Required Apparatus & Chemicals
Laboratory Apparatus
- UV-Vis spectrophotometer
- Separating funnels 125 mL
- Volumetric flasks 50 mL
- Pipettes
- Cuvettes
Chemical Reagents
- Ni standard solution (10 mg L⁻¹)
- Dimethylglyoxime (1% in ethanol)
- Ammonia solution (1:1)
- Bromine water
- Chloroform
- Unknown nickel sample
Step-by-Step Practical Procedure
- Place 0-5 mL Ni standard in separating funnels (0-1 mg L⁻¹ range after dilution).
- Add bromine water, then ammonia to make the solution ammoniacal.
- Add 5 mL DMG solution and shake with 10 mL chloroform for 2 min.
- Separate the lower chloroform layer into a 50 mL flask; repeat extraction.
- Dilute the combined extract to 50 mL with chloroform; treat unknown identically.
- Zero at 465 nm with chloroform and read absorbances.
Observations & Expected Results
Red complex collects in the lower chloroform layer; organic-phase absorbance at 465 nm is linear with nickel; aqueous layer remains nearly colourless.
Worked Stoichiometric Calculations
Problem: A steel digest (1.000 g to 100 mL) aliquot extracted to 50 mL CHCl3 gives A = 0.472 at 465 nm (ε = 1.70 × 10⁴, l = 1 cm). The aliquot was the full 100 mL. Find Ni in ppm.
Working: c = 0.472/1.70 × 10⁴ = 2.78 × 10⁻⁵ mol L⁻¹. Mass in 0.050 L = 2.78 × 10⁻⁵ × 0.050 × 58.69 = 8.15 × 10⁻⁵ g = 0.0815 mg. ppm = 0.0815 mg/1.000 g = 81.5 ppm.
Safety Precautions & Hazard Control
- Use chloroform in a fume cupboard; avoid inhalation.
- Shake the funnel gently with frequent venting to release pressure.
- Keep the ammoniacal pH the same for standards and sample.
- Dry the extract over anhydrous Na2SO4 if it appears cloudy.
Waste Disposal Protocol
Collect all chloroform extracts in the halogenated organic waste bottle, never down the drain.
Viva Voce Oral Defense Questions & Answers
Q: Why is nickel extracted into chloroform?
A: The neutral Ni(DMG)2 chelate partitions into the organic phase, separating Ni from aqueous interferences and intensifying the colour in a small volume.
Q: Why is bromine water added before DMG?
A: It oxidises interfering Co(II) and ensures nickel is in the correct state for quantitative chelate formation.
Q: Why is the solution made ammoniacal?
A: The DMG complex forms quantitatively in mildly alkaline medium; in acid the chelate does not precipitate.