CHEMVEN

Copper in Copper Sulfate Pentahydrate by Electrogravimetry

Check the purity of CuSO4·5H2O by electrodepositing its copper.

Level: UniversitySafety: SafeTime: 2 h
Aim of Experiment: Check the purity of CuSO4·5H2O by electrodepositing its copper.

Theoretical Foundations

CuSO4·5H2O dissolves to give Cu2+, which deposits quantitatively: Cu2+ + 2e- → Cu(s). Pure salt contains 63.55/249.68 = 25.45% Cu. The cathode mass gain gives % Cu directly; comparison with theory gives the purity and demonstrates electrogravimetry on a clean, single-salt system.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Analytical balance
  • Platinum electrodes
  • DC power supply
  • 250 mL beaker
  • Oven
  • Desiccator

Chemical Reagents

  • Copper sulfate pentahydrate sample
  • Sulfuric acid, dilute
  • Distilled water
  • Ethanol

Step-by-Step Practical Procedure

  1. Weigh the Pt cathode (mass A).
  2. Weigh accurately 1.0 g CuSO4·5H2O; dissolve in 150 mL water with 5 mL dilute H2SO4.
  3. Electrolyse at 1.5-2 A with stirring for 45 minutes.
  4. Test for completeness on a fresh cathode area.
  5. Wash the cathode with the current on, rinse with ethanol, dry at 110 C.
  6. Weigh (mass B); calculate % Cu and purity.

Observations & Expected Results

Blue solution decolourises as pink copper builds up; typical deposit about 0.25 g from 1 g salt.

Worked Stoichiometric Calculations

Problem: 1.000 g of salt gave a cathode gain of 0.2545 g Cu. Calculate % Cu and purity. (Theoretical = 25.45%)

Working: % Cu = (0.2545/1.000) × 100 = 25.45%. Purity = 100.0% — the salt meets its specification.

Safety Precautions & Hazard Control

  • Keep the current on while washing the cathode.
  • Acidify with H2SO4 for good conductivity.
  • Dry the cathode fully; trapped water gives high results.

Waste Disposal Protocol

Depleted electrolyte to heavy-metal waste.

Viva Voce Oral Defense Questions & Answers

Q: Use Faraday's law to predict the theoretical deposit for 2 A × 30 min.

A: Q = 3600 C; moles e- = 3600/96485 = 0.0373; moles Cu = 0.01866; mass = 0.01866 × 63.55 = 1.186 g.

Q: Why add sulfuric acid to the bath?

A: It provides conductivity, prevents hydrolysis of Cu2+ and keeps the anode reaction clean (oxygen evolution).

← Back to Experiments Directory