Double Precipitation for High-Purity Ni(DMG)2
Show that reprecipitation (double precipitation) removes coprecipitated impurities from Ni(DMG)2.
Theoretical Foundations
The first precipitate always carries adsorbed foreign salts. Dissolving it in hot dilute HCl (Ni(HDMG)2 + 2H+ → Ni2+ + 2 H2DMG) and reprecipitating with ammonia gives a much purer product, because impurities are diluted into a fresh solution and largely stay dissolved the second time. Comparing single vs double precipitation on identical aliquots quantifies the purification.
Required Apparatus & Chemicals
Laboratory Apparatus
- Analytical balance
- Two 400 mL beakers
- Hot plate
- Sintered-glass crucibles
- Oven
- Desiccator
Chemical Reagents
- Nickel alloy sample with soluble impurities
- Hydrochloric acid, dilute
- Dimethylglyoxime solution, 1% in ethanol
- Ammonia solution, dilute
- Distilled water
Step-by-Step Practical Procedure
- Dissolve two identical 0.4000 g portions of alloy and precipitate Ni(DMG)2 in both as usual.
- Filter beaker A directly: wash, dry and weigh (single precipitation).
- Filter beaker B, then dissolve its precipitate in hot dilute HCl.
- Reprecipitate B with ammonia, filter, wash, dry at 150 C to constant mass and weigh.
- Compare the two masses and calculated % Ni.
Observations & Expected Results
Both precipitates are scarlet; the reprecipitated one is slightly lighter, showing impurity removal.
Worked Stoichiometric Calculations
Problem: Single precipitation gave 0.7950 g (apparent 40.39% Ni); double precipitation gave 0.7865 g. True value 39.9% Ni. Calculate the % Ni from the double precipitation.
Working: Mass Ni = 0.7865 × 0.2032 = 0.1598 g. % Ni = (0.1598/0.4000) × 100 = 39.95%, essentially the true value; single precipitation was 0.5% high from impurities.
Safety Precautions & Hazard Control
- Dissolve the first precipitate completely before reprecipitating.
- Wash the second precipitate thoroughly.
- Keep conditions identical except for the reprecipitation step.
Waste Disposal Protocol
Nickel filtrates to heavy-metal waste.
Viva Voce Oral Defense Questions & Answers
Q: Why does reprecipitation purify the product?
A: Impurities adsorbed on the first precipitate are released into a fresh solution on redissolution; at their now-low concentration they stay dissolved while the nickel reprecipitates.
Q: When is double precipitation mandatory?
A: When the precipitate is known to coprecipitate significant impurities, e.g. MgNH4PO4 carrying Ca2+, or any chelate formed in a high-salt matrix.