CHEMVEN

Photodecomposition of AgCl: Quantitative Light-Damage Study

Measure the mass loss when AgCl is exposed to sunlight and relate it to the photodecomposition reaction.

Level: UniversitySafety: SafeTime: 2 h
Aim of Experiment: Measure the mass loss when AgCl is exposed to sunlight and relate it to the photodecomposition reaction.

Theoretical Foundations

Silver chloride is photosensitive: 2AgCl(s) → 2Ag(s) + Cl2(g). Chlorine gas escapes, so the solid loses mass; the residue darkens from white to violet-grey. The fractional mass loss on complete decomposition equals M_Cl2/(2 × M_AgCl) = 70.90/286.64 = 0.2473, so the observed loss directly measures the fraction decomposed.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Analytical balance
  • Two weighed sintered-glass crucibles
  • Sunlight or UV lamp
  • Dark cupboard
  • Oven

Chemical Reagents

  • Silver chloride precipitate (freshly prepared)
  • Nitric acid, very dilute (rinsing)
  • Distilled water

Step-by-Step Practical Procedure

  1. Prepare AgCl by mixing AgNO3 and NaCl solutions in the dark; filter and wash.
  2. Divide the damp precipitate between two weighed crucibles; dry both at 150 C to constant mass in the dark and weigh.
  3. Expose crucible A to bright sunlight for 2 hours; keep crucible B in a dark cupboard.
  4. Reweigh both crucibles.
  5. Calculate the mass loss of A and the % decomposition.

Observations & Expected Results

The exposed precipitate turns violet-grey and loses mass; the dark control stays white with unchanged mass.

Worked Stoichiometric Calculations

Problem: 0.4000 g of AgCl exposed to sunlight lost 0.0200 g. Calculate the % of AgCl decomposed. (Fractional loss on full decomposition = 0.2473)

Working: Fractional loss observed = 0.0200/0.4000 = 0.0500. % decomposed = (0.0500/0.2473) × 100 = 20.2%.

Safety Precautions & Hazard Control

  • Prepare and dry the precipitate in the dark before the exposure step.
  • Handle the UV lamp/sunlight with eye protection.
  • Weigh quickly; the decomposed surface can re-adsorb moisture.

Waste Disposal Protocol

Silver residues collected for recovery.

Viva Voce Oral Defense Questions & Answers

Q: Write the photodecomposition reaction of AgCl.

A: 2AgCl(s) → 2Ag(s) + Cl2(g) under light.

Q: How does this experiment justify the 'work in the dark' rule?

A: Even 2 hours of sunlight decomposed 20% of the AgCl here; in analysis such decomposition causes serious negative errors, hence foil-wrapped glassware and subdued light.

Q: What is the photographic relevance?

A: The same light sensitivity is the basis of black-and-white photography, where AgBr/AgCl in film is reduced to metallic silver specks.

← Back to Experiments Directory