Bismuth (Bi) — Element 83

Standard Atomic Weight: 208.98 u · Electronic Configuration: [Xe] 4f14 5d10 6s2 6p3

Z = 83POST-TRANSITION METALPeriod 6, Group 15p-block

Fundamental Periodic Properties

Atomic Number (Z)83
Chemical SymbolBi
Standard Atomic Weight208.98 u (IUPAC CIAAW)
CategoryPost-transition metal
Group, Period, BlockGroup 15, Period 6, p-block
Electron Configuration[Xe] 4f14 5d10 6s2 6p3
Electrons per Shell2,8,18,32,18,5
Common Oxidation States+3
State at STPsolid
Electronegativity (Pauling)2.02
1st Ionization Energy7.286 eV
Atomic Radius148 pm
Crystal Structurerhombohedral

Discovery & Historical Context

Discovered: ~1400s by Described by Basil Valentine

Name Origin: German wismut

Everyday Applications & Technological Role

Pepto-Bismol, cosmetics, lead-free solder

Key Scientific Facts

← Previous: Element 82 Back to Periodic Table Next: Element 84 →