Standard Atomic Weight: 9.012 u · Electronic Configuration: [He] 2s2

Z = 4ALKALINE EARTHPeriod 2, Group 2s-block

Fundamental Periodic Properties

Atomic Number (Z)4
Chemical SymbolBe
Standard Atomic Weight9.012 u (IUPAC CIAAW)
CategoryAlkaline earth
Group, Period, BlockGroup 2, Period 2, s-block
Electron Configuration[He] 2s2
Electrons per Shell2,2
Common Oxidation States+2
State at STPsolid
Electronegativity (Pauling)1.57
1st Ionization Energy9.323 eV
Atomic Radius96 pm
Crystal Structurehcp

Discovery & Historical Context

Discovered: 1798 by Louis-Nicolas Vauquelin

Name Origin: Greek beryllos (beryl)

Everyday Applications & Technological Role

Aerospace parts, X-ray windows (toxic dust!)

Key Scientific Facts