Ruthenium (Ru) — Element 44

Standard Atomic Weight: 101.07 u · Electronic Configuration: [Kr] 4d7 5s1

Z = 44TRANSITION METALPeriod 5, Group 8d-block

Fundamental Periodic Properties

Atomic Number (Z)44
Chemical SymbolRu
Standard Atomic Weight101.07 u (IUPAC CIAAW)
CategoryTransition metal
Group, Period, BlockGroup 8, Period 5, d-block
Electron Configuration[Kr] 4d7 5s1
Electrons per Shell2,8,18,15,1
Common Oxidation States+4, +3
State at STPsolid
Electronegativity (Pauling)2.2
1st Ionization Energy7.361 eV
Atomic Radius146 pm
Crystal Structurehcp

Discovery & Historical Context

Discovered: 1844 by Karl Claus

Name Origin: Latin Ruthenia (Russia)

Everyday Applications & Technological Role

Electrical contacts, catalysts, fountain-pen nibs