CHEMVEN

Polymer Fundamentals — Chains, Addition vs Condensation

How monomers become macromolecules, and how chain length is measured.

MATERIALSLevel: IntermediateAcademic Reference

Overview & Foundations

A polymer is a macromolecule built from repeating units (mers) joined in long chains. Addition polymerization links monomers with C=C double bonds (e.g. ethylene → polyethylene) with no by-product, initiated by radicals, cations or Ziegler–Natta catalysts; condensation polymerization joins bifunctional monomers (e.g. diacid + diol → polyester) with loss of a small molecule such as water, and the chain grows stepwise so high molar mass requires very high conversion.

Chain length is described by averages: the number-average molar mass Mn = ΣNiMi/ΣNi and the weight-average Mw = ΣNiMi²/ΣNiMi. Their ratio PDI = Mw/Mn (polydispersity index) measures breadth — PDI = 1 is perfectly uniform, commercial polymers are 1.5–3. The degree of polymerization DP = Mn / M₀ where M₀ is the repeat-unit molar mass.

Core Chemical Concepts

Governing Formulas & Laws

Mn = ΣNiMi/ΣNi; Mw = ΣNiMi²/ΣNiMi
Averages
PDI = Mw/Mn
Dispersity
DP = Mn/M₀
Degree of polymerization

Worked Numerical Examples

A polystyrene sample has Mn = 260,000 g/mol. What is the average degree of polymerization?
Repeat unit = styrene C₈H₈, M₀ = 8(12.01)+8(1.008) = 104.15 g/mol. DP = 260,000 / 104.15 ≈ 2,496 ≈ 2.5×10³ repeat units per chain.

Industrial & Laboratory Applications

Common Student Misconceptions

Mn and Mw are different averages — do not confuse them; Mw weights long chains more
Condensation needs >99% conversion for long chains (Carothers equation)
PDI can never be less than 1

Everyday Life & Real-World Relevance

Practice & Review Questions

If Mw = 150,000 and PDI = 1.5, what is Mn?
Mn = Mw/PDI = 100,000 g/mol.
Why does condensation polymerization need near-complete conversion?
Step growth: chains grow by joining oligomers, so DP = 1/(1−p); only at p → 1 do long chains form.

Scholarly Literature & References

← Back to Materials Hub · All Encyclopedia Topics