Carbon Allotropes — Graphene, Nanotubes, Fullerenes
One element, many super-materials: from pencil lead to the strongest fiber known.
Overview & Foundations
Carbon's allotropes differ only in how sp² or sp³ carbons are networked. Graphene is a single honeycomb sheet of sp² carbon (C–C 0.142 nm) — a zero-gap semiconductor with electron mobility ~200,000 cm²/V·s and tensile strength ~130 GPa. Rolling it gives carbon nanotubes: armchair tubes are metallic, zigzag/chiral tubes are semiconducting depending on the (n,m) indices; multi-walled tubes reach strengths ~60 GPa. Closing the sheet gives fullerenes like C₆₀ (buckminsterfullerene, truncated icosahedron).
Contrast diamond (sp³, tetrahedral, 3.51 g/cm³, hardest natural material, electrical insulator) with graphite (sp² layers held by van der Waals forces, soft, conducts in-plane). Same atoms — bonding geometry decides everything.
Core Chemical Concepts
- Graphene: single sp² sheet, 0.142 nm bonds, extraordinary strength/conductivity
- CNT chirality (n,m): armchair = metallic; others mostly semiconducting
- C₆₀ fullerene: 60 carbons, soccer-ball cage
- Diamond (sp³, hard, insulator) vs graphite (sp² layers, soft, conductor)
Governing Formulas & Laws
Bond lengthGrapheneDiamondWorked Numerical Examples
Industrial & Laboratory Applications
- CNT-reinforced composites, conductive inks, battery electrodes
- Graphene membranes, flexible electronics, sports equipment
Common Student Misconceptions
Everyday Life & Real-World Relevance
- Graphene/CNT/fullerene structures
- sp² vs sp³ property contrast
- Chirality → electronic behavior