Spiro-OMeTAD (C81H68N4O8)

CAS Registry Number: 207739-72-8 · Standard Molar Mass: 1225.45 g/mol

SOLIDCAS: 207739-72-8MW: 1225.45 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC NameN2,N2,N2',N2',N7,N7,N7',N7'-Octakis(4-methoxyphenyl)-9,9'-spirobi[9H-fluorene]-2,2',7,7'-tetramine
Chemical FormulaC81H68N4O8
CAS Registry Number207739-72-8
Molar Mass1225.45 g/mol
State of Matter (STP)solid
Melting Point
Boiling Point
Categorymaterials
GHS Hazard CategoryNon-hazardous

Everyday & Industrial Uses

The standard hole-transport material of perovskite solar cells.

Chemical Notes & Behavior

A spiro-centred glassy molecule; it needs dopants to conduct, which costs stability.