Magnesium oxide (MgO)
CAS Registry Number: 1309-48-4 · Standard Molar Mass: 40.30 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).
Chemical & Physical Constants
| IUPAC Name | Oxomagnesium |
|---|---|
| Chemical Formula | MgO |
| CAS Registry Number | 1309-48-4 |
| Molar Mass | 40.30 g/mol |
| State of Matter (STP) | solid |
| Melting Point | 2800 °C (NIOSH, 2024) |
| Boiling Point | 3600 °C (NIOSH, 2024) |
| Category | academic |
| GHS Hazard Category | Non-hazardous |
Everyday & Industrial Uses
Refractory furnace lining; antacid (magnesia); cement component.
Chemical Notes & Behavior
Periclase — melts above 2,800 °C and slowly slakes in moist air.