Lithium fluoride (LiF)

CAS Registry Number: 7789-24-4 · Standard Molar Mass: 25.94 g/mol

SOLIDCAS: 7789-24-4MW: 25.94 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC NameLithium fluoride
Chemical FormulaLiF
CAS Registry Number7789-24-4
Molar Mass25.94 g/mol
State of Matter (STP)solid
Melting Point848.2 °C
Boiling Point1673 °C
Categorymaterials
GHS Hazard CategoryToxic if swallowed

Everyday & Industrial Uses

Radiation dosimeters, ultraviolet optics and a key SEI component in lithium batteries.

Chemical Notes & Behavior

Transmits further into the ultraviolet than any other common solid; very sparingly soluble.