Gallium(III) oxide (Ga2O3)

CAS Registry Number: 12024-21-4 · Standard Molar Mass: 187.44 g/mol

SOLIDCAS: 12024-21-4MW: 187.44 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC NameDigallium trioxide
Chemical FormulaGa2O3
CAS Registry Number12024-21-4
Molar Mass187.44 g/mol
State of Matter (STP)solid
Melting Point
Boiling Point
Categorymaterials
GHS Hazard CategoryNon-hazardous

Everyday & Industrial Uses

Ultra-wide-bandgap power electronics and solar-blind ultraviolet detectors.

Chemical Notes & Behavior

Band gap near 4.8 eV — wider than GaN or SiC — but it conducts heat poorly.