CHEMVEN

Ethylene carbonate (C3H4O3)

CAS Registry Number: 96-49-1 · Standard Molar Mass: 88.06 g/mol

SOLIDCAS: 96-49-1MW: 88.06 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC Name1,3-Dioxolan-2-one
Chemical FormulaC3H4O3
CAS Registry Number96-49-1
Molar Mass88.06 g/mol
State of Matter (STP)solid
Melting Point36.4 °C
Boiling Point248 °C
Categorymaterials
GHS Hazard CategoryEye damage, Organ toxicity

Everyday & Industrial Uses

Core lithium-ion electrolyte solvent — it builds the protective SEI film on graphite.

Chemical Notes & Behavior

Melts at 36 °C, so it is always blended with thinner carbonates to flow.