Cobalt(II,III) oxide (Co3O4)
CAS Registry Number: 1308-06-1 · Standard Molar Mass: 240.80 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).
Chemical & Physical Constants
| IUPAC Name | Tricobalt tetraoxide |
|---|---|
| Chemical Formula | Co3O4 |
| CAS Registry Number | 1308-06-1 |
| Molar Mass | 240.80 g/mol |
| State of Matter (STP) | solid |
| Melting Point | |
| Boiling Point | |
| Category | materials |
| GHS Hazard Category | Sensitizer |
Everyday & Industrial Uses
Oxidation catalysts, gas sensors, pigments and battery-electrode research.
Chemical Notes & Behavior
Black spinel holding Co(II) and Co(III) in the same lattice.