Cobalt antimonide (CoSb3)

CAS Registry Number: 12052-42-5 · Standard Molar Mass: 424.21 g/mol

SOLIDCAS: 12052-42-5MW: 424.21 g/mol
Safety Notice: For educational reference only. Always consult the official Safety Data Sheet (SDS).

Chemical & Physical Constants

IUPAC NameCobalt antimonide
Chemical FormulaCoSb3
CAS Registry Number12052-42-5
Molar Mass424.21 g/mol
State of Matter (STP)solid
Melting Point
Boiling Point
Categorymaterials
GHS Hazard CategoryHarmful

Everyday & Industrial Uses

Skutterudite thermoelectrics for mid-temperature waste-heat recovery.

Chemical Notes & Behavior

Its cage lattice lets filler atoms rattle, blocking heat flow while electrons pass.